Oxidation resistance evaluation (calo test crater after being held for 1 hour in the atmosphere at 1,100°C)
Oxidation resistance tests conducted under NACHI standards showed GSX II coating limits oxidation to 0.3µm from the surface, whereas coating products of competitors resulted in total oxidation of the coating layer.
Comparison of wear after grooving 10m with S50C